Nan blog sa a, nou prezante rezèv la nanFittings 254SMO fabrike nan estanda ASME B16.9. 254SMO, ke yo rele tou UNS S31254 oswa Alloy 254, se yon asye pur super austenitic li te ye pou rezistans eksepsyonèl korozyon li nan anviwònman difisil. Koup ak espesifikasyon solid nan ASME B16.9, ekipman sa yo ofri solisyon pou pwosesis chimik, lwil oliv ak gaz, ak aplikasyon pou maren.

Apèsi sou materyèl 254SMO
254SMO se yon wo-alyaj austenitic Nerjaveèi ki fèt pou rezistans siperyè nan twou, kowozyon nan fant, ak krak korozyon estrès, patikilyèman nan klori-kondisyon ki rich ak asid.
Konpozisyon chimik li gen ladan apeprè 19.5-20.5% chromium, 17.5-18.5% nikèl, 6.0-6.5% molybdène, 0.18-0.22% nitwojèn, ak 0.50-1.00% kwiv, ak yon kontni kabòn ki ba (max 0.02%) pou minimize presipitasyon carbure.

Mekanikman, li montre yon fòs rupture minimòm de 650-680 MPa, fòs sede 300 MPa, ak yon elongasyon 35%, ki fè li tou de fò ak duktil. Pwopriyete sa yo soti nan amelyorasyon molybdène ak nitwojèn li yo, reyalize yon Pitting Resistance Ekivalan Nimewo (PREN) ki pi gran pase oswa egal a 42.5, byen lwen depase klas estanda ostenitik tankou 316L.
Lè fabrike nan ekipman anba ASME B16.9, 254SMO asire konfòmite ak evalyasyon presyon, tolerans, ak egzijans tès, sa ki fè li ideyal pou gwo -sistèm kanalizasyon entegrite.
254SMO Buttweld Fittings Kalite
Manifakti yo bay ekipman 254SMO buttweld pou fasilite chanjman direksyon, koneksyon branch, ak tranzisyon dyamèt nan sistèm kanalizasyon. Sa yo se sitou fabrike nan ASTM A403 / ASME SA403, spesifikasyon estanda pou ekipman tiyo asye pur austenitic.

Koud:Yo itilize pou chanje direksyon koule. Sa yo disponib nan ang estanda 90-degre ak 45-degre, ak reyon long (LR) ak reyon kout (SR). Long Radius koud yo gen yon dimansyon sant-a-fas 1.5 fwa gwosè tiyo nominal la, pandan y ap koud kout reyon yo gen yon reyon ki egal a gwosè tiyo a. Koud espesyalize tankou 3D, 5D, ak 180-degre viraj retounen yo disponib tou pou kondisyon espesifik koule.
Tees:Sa yo pèmèt pou koneksyon branch. Equal Tees gen tout twa plòg nan menm gwosè a, pandan y ap Reducing Tees gen yon priz branch ki pi piti pase kouri prensipal la.
Rediksyon:Fasilite yon chanjman nan dyamèt tiyo. Reduktè konsantrik yo simetrik, ak yon liy santral komen, tandiske redukteur ekssantrik yo gen yon sèl bò plat, yo itilize pou kenbe swa anwo oswa anba nivo tiyo a.
bouchon:Sa yo pèmanan sele fen yon tiyo.
Bouch bout (Lap Joint Stub Ends):Itilize ak bride jwenti pou kreye yon pwen koneksyon boulon nan sistèm nan.
Kwaze:Bay koneksyon pou kat tiyo rankontre nan yon pwen.
254SMO Fittings Spesifikasyon ak dimansyon
Espesifikasyon pou ekipman 254SMO ASME B16.9 konfòme yo ak ASTM A403 WP-S31254 pou asye pur austenitic fòje, ak epesè miray matche ak Orè 10S jiska 160 oswa XXS, tou depann de kondisyon presyon.
REMAK JENERAL: Tout dimansyon yo an milimèt.
Dimansyon Tees Dwat Ak kwa
|
Gwosè tiyo nominal (NPS) |
DN |
Dyamèt deyò nan Bevel |
Sant-pou-Fen |
|
|
Kouri, C |
Outlet, M [Nòt (1) ak (2)] |
|||
|
1/2 |
15 |
21.3 |
25 |
25 |
|
3/4 |
20 |
26.7 |
29 |
29 |
|
1 |
25 |
33.4 |
38 |
38 |
|
1 1/4 |
32 |
42.2 |
48 |
48 |
|
1 1/2 |
40 |
48.3 |
57 |
57 |
|
2 |
50 |
60.3 |
64 |
64 |
|
2 1/2 |
65 |
73.0 |
76 |
76 |
|
3 |
80 |
88.9 |
86 |
86 |
|
3 1/2 |
90 |
101.6 |
95 |
95 |
|
4 |
100 |
114.3 |
105 |
105 |
|
5 |
125 |
141.3 |
124 |
124 |
|
6 |
150 |
168.3 |
143 |
143 |
|
8 |
200 |
219.1 |
178 |
178 |
|
10 |
250 |
273.0 |
216 |
216 |
|
12 |
300 |
323.8 |
254 |
254 |
|
14 |
350 |
355.6 |
279 |
279 |
|
16 |
400 |
406.4 |
305 |
305 |
|
18 |
450 |
457 |
343 |
343 |
|
20 |
500 |
508 |
381 |
381 |
|
22 |
550 |
559 |
419 |
419 |
|
24 |
600 |
610 |
432 |
432 |
|
26 |
650 |
660 |
495 |
495 |
|
28 |
700 |
711 |
521 |
521 |
|
30 |
750 |
762 |
559 |
559 |
|
32 |
800 |
813 |
597 |
597 |
|
34 |
850 |
864 |
635 |
635 |
|
36 |
900 |
914 |
673 |
673 |
|
38 |
950 |
965 |
711 |
711 |
|
40 |
1000 |
1016 |
749 |
749 |
|
42 |
1050 |
1067 |
762 |
711 |
|
44 |
1100 |
1118 |
813 |
762 |
|
46 |
1150 |
1168 |
851 |
800 |
|
48 |
1200 |
1219 |
889 |
838 |
Dimansyon Koud Reyon Kout
|
Gwosè tiyo nominal (NPS) |
DN |
Dyamèt deyò nan bizote |
Sant-pou-Fen, A |
|
1 |
25 |
33.4 |
25 |
|
1 1/4 |
32 |
42.2 |
32 |
|
1 1/2 |
40 |
48.3 |
38 |
|
2 |
50 |
60.3 |
51 |
|
2 1/2 |
65 |
73.0 |
64 |
|
3 |
80 |
88.9 |
76 |
|
3 1/2 |
90 |
101.6 |
89 |
|
4 |
100 |
114.3 |
102 |
|
5 |
125 |
141.3 |
127 |
|
6 |
150 |
168.3 |
152 |
|
8 |
200 |
219.1 |
203 |
|
10 |
250 |
273.0 |
254 |
|
12 |
300 |
323.8 |
305 |
|
14 |
350 |
355.6 |
356 |
|
16 |
400 |
406.4 |
406 |
|
18 |
450 |
457 |
457 |
|
20 |
500 |
508 |
508 |
|
22 |
550 |
559 |
559 |
|
24 |
600 |
610 |
610 |
Dimansyon nan reyon kout 180 Deg Returns
|
Nominal Tiyo Gwosè (NPS) |
DN |
Deyò Dyamèt nan Bevel |
Sant- pou - Sant, O |
Retounen- nan- figi, K |
|
1 |
25 |
33.4 |
51 |
41 |
|
1 1/4 |
32 |
42.2 |
64 |
52 |
|
1 1/2 |
40 |
48.3 |
76 |
62 |
|
2 |
50 |
60.3 |
102 |
81 |
|
2 1/2 |
65 |
73.0 |
127 |
100 |
|
3 |
80 |
88.9 |
152 |
121 |
|
3 1/2 |
90 |
101.6 |
178 |
140 |
|
4 |
100 |
114.3 |
203 |
159 |
|
5 |
125 |
141.3 |
254 |
197 |
|
6 |
150 |
168.3 |
305 |
237 |
|
8 |
200 |
219.1 |
406 |
313 |
|
10 |
250 |
273.0 |
508 |
391 |
|
12 |
300 |
323.8 |
610 |
467 |
|
14 |
350 |
355.6 |
711 |
533 |
|
16 |
400 |
406.4 |
813 |
610 |
|
18 |
450 |
457 |
914 |
686 |
|
20 |
500 |
508 |
1016 |
762 |
|
22 |
550 |
559 |
1118 |
838 |
|
24 |
600 |
610 |
1219 |
914 |
Dimansyon nan Diminye Tees priz ak Diminye kwa priz
|
Nominal Tiyo Gwosè (NPS) |
DN |
Deyò Dyamèt nan Bizote Kouri Debouche |
Sant-pou-Fen |
||
|
Kouri, C |
priz, M [Remak (1)] |
||||
|
1/2 x 1/2 x 3/8 |
15 × 15 × 10 |
21.3 |
17.3 |
25 |
25 |
|
1/2 x1/2 x 1/4 |
15 × 15 × 8 |
21.3 |
13.7 |
25 |
25 |
|
3/4 x 3/4 x1/2 |
20 × 20 × 15 |
26.7 |
21.3 |
29 |
29 |
|
3/4 x 3/4 x 3/8 |
20 × 20 × 10 |
26.7 |
17.3 |
29 |
29 |
|
1 × 1 x 3/4 |
25 × 25 × 20 |
33.4 |
26.7 |
38 |
38 |
|
1 × 1 x 1/2 |
25 × 25 × 15 |
33.4 |
21.3 |
38 |
38 |
|
1 1/4 x 1 1/4 × 1 |
32 × 32 × 25 |
42.2 |
33.4 |
48 |
48 |
|
1 1/4 × 1 1/4 × 3/4 |
32 × 32 × 20 |
42.2 |
26.7 |
48 |
48 |
|
1 1/4 x 1 1/4 x 1/2 |
32 × 32 × 15 |
42.2 |
21.3 |
48 |
48 |
|
1 1/2 x 1 1/2 x 1/4 |
40 × 40 × 32 |
48.3 |
42.2 |
57 |
57 |
|
1 1/2 x 1 1/2 × 1 |
40 × 40 × 25 |
48.3 |
33.4 |
57 |
57 |
|
1 1/2 x 1 1/2 x 3/4 |
40 × 40 × 20 |
48.3 |
26.7 |
57 |
57 |
|
1 1/2 x 1 1/2x 1/2 |
40 × 40 × 15 |
48.3 |
21.3 |
57 |
57 |
|
2 × 2 × 1 1/2 |
50 × 50 × 40 |
60.3 |
48.3 |
64 |
60 |
|
2 × 2 × 1 1/4 |
50 × 50 × 32 |
60.3 |
42.2 |
64 |
57 |
|
2 × 2 × 1 |
50 × 50 × 25 |
60.3 |
33.4 |
64 |
51 |
|
2 × 2 × 3/4 |
50 × 50 × 20 |
60.3 |
26.7 |
64 |
44 |
|
2 1/2 x 2 1/2 × 2 |
65 × 65 × 50 |
73.0 |
60.3 |
76 |
70 |
|
2 1/2 x 2 1/2 x 1 1/2 |
65 × 65 × 40 |
73.0 |
48.3 |
76 |
67 |
|
2 1/2 × 2 1/2 × 1 1/4 |
65 × 65 × 32 |
73.0 |
42.2 |
76 |
64 |
|
2 1/2 × 2 1/2 × 1 |
65 × 65 × 25 |
73.0 |
33.4 |
76 |
57 |
|
3 × 3 × 2 1/2 |
80 × 80 × 65 |
88.9 |
73.0 |
86 |
83 |
|
3 × 3 × 2 |
80 × 80 × 50 |
88.9 |
60.3 |
86 |
76 |
|
3 × 3 × 1 1/2 |
80 × 80 × 40 |
88.9 |
48.3 |
86 |
73 |
|
3 × 3 × 1 1/4 |
80 × 80 × 32 |
88.9 |
42.2 |
86 |
70 |
|
3 1/2 x 3 1/2 × 3 |
90 × 90 × 80 |
101.6 |
88.9 |
95 |
92 |
|
3 1/2 × 3 1/2 × 2 1/2 |
90 × 90 × 65 |
101.6 |
73.0 |
95 |
89 |
|
3 1/2 × 3 1/2 × 2 |
90 × 90 × 50 |
101.6 |
60.3 |
95 |
83 |
|
3 1/2 × 3 1/2 × 1 1/2 |
90 × 90 × 40 |
101.6 |
48.3 |
95 |
79 |
|
4 × 4 × 3 1/2 |
100 × 100 × 90 |
114.3 |
101.6 |
105 |
102 |
|
4 × 4 × 3 |
100 × 100 × 80 |
114.3 |
88.9 |
105 |
98 |
|
4 × 4 × 2 1/2 |
100 × 100 × 65 |
113.3 |
73.0 |
105 |
95 |
|
4 × 4 × 2 |
100 × 100 × 50 |
114.3 |
60.3 |
105 |
89 |
|
4 × 4 × 1 1/2 |
100 × 100 × 40 |
114.3 |
48.3 |
105 |
86 |
|
5 × 5 × 4 |
125 × 125 × 100 |
141.3 |
114.3 |
125 |
117 |
|
5 × 5 × 3 1/2 |
125 × 125 × 90 |
141.3 |
101.6 |
124 |
114 |
|
5 × 5 × 3 |
125 × 125 × 80 |
141.3 |
88.9 |
124 |
111 |
|
5 × 5 × 2 1/2 |
125 × 125 × 65 |
141.3 |
73.0 |
124 |
108 |
|
5 × 5 × 2 |
125 × 125 × 50 |
141.3 |
60.3 |
124 |
105 |
Dimansyon nan redukteur
|
Tiyo nominal Gwosè (NPS) |
DN |
Deyò Dyamèt nan Bizote |
Fen-a-Fen, H |
Tiyo nominal Gwosè (NPS) |
DN |
Deyò Dyamèt nan Bizote |
Fen-a-Fen, H |
||
|
Gwo Fen |
Ti Fen |
Gwo Fen |
Ti Fen |
||||||
|
3/4 x 1/2 |
20 ×15 |
26.7 |
21.3 |
38 |
5 × 4 |
125 ×100 |
141.3 |
114.3 |
127 |
|
3/4 x 3/8 |
20 ×10 |
26.7 |
17.3 |
38 |
5 × 3 1/2 |
125 ×90 |
141.3 |
101.6 |
127 |
|
1 × 3/4 |
25 ×20 |
33.4 |
26.7 |
51 |
5 × 3 |
125 ×80 |
141.3 |
88.9 |
127 |
|
1 × 1/2 |
25 ×15 |
33.4 |
21.3 |
51 |
5 × 2 1/2 |
125 ×65 |
141.3 |
73.0 |
127 |
|
1 1/4 × 1 |
32 ×25 |
42.2 |
33.4 |
51 |
5 × 2 |
125 × 50 |
141.3 |
60.3 |
127 |
|
1 1/4 ×3/4 |
32 ×20 |
42.2 |
26.7 |
51 |
6 × 5 |
150 ×125 |
168.3 |
141.3 |
140 |
|
1 1/4 x 1/2 |
32 ×15 |
42.2 |
21.3 |
51 |
6 × 4 |
150 ×100 |
168.3 |
114.3 |
140 |
|
1 1/2 x 1 1/4 |
40 ×32 |
48.3 |
42.2 |
64 |
6 × 3 1/2 |
150 ×90 |
168.3 |
101.6 |
140 |
|
1 1/2 × 1 |
40 ×25 |
48.3 |
33.4 |
64 |
6 × 3 |
150 ×80 |
168.3 |
88.9 |
140 |
|
1 1/2 x 3/4 |
40 ×20 |
48.3 |
26.7 |
64 |
6 × 2 1/2 |
150 ×65 |
168.3 |
73.0 |
140 |
|
1 1/2 x 1/2 |
40 ×15 |
48.3 |
21.3 |
64 |
8 × 6 |
200 ×150 |
219.1 |
168.3 |
152 |
|
2 ×1 1/2 |
50 ×40 |
60.3 |
48.3 |
76 |
8 × 5 |
200 ×125 |
219.1 |
141.3 |
152 |
|
2 ×1 1/4 |
50 ×32 |
60.3 |
42.2 |
76 |
8 × 4 |
200 ×100 |
219.1 |
114.3 |
152 |
|
2 × 1 |
50 ×25 |
60.3 |
33.4 |
76 |
8 × 3 1/2 |
200 ×90 |
219.1 |
101.6 |
152 |
|
2 ×3/4 |
50 ×20 |
60.3 |
26.7 |
76 |
10 × 8 |
250 ×200 |
273.0 |
219.1 |
178 |
|
2 1/2 x 2 |
65 ×50 |
73.0 |
60.3 |
89 |
10 × 6 |
250 ×150 |
273.0 |
168.3 |
178 |
|
2 1/2 x 1 1/2 |
65 ×40 |
73.0 |
48.3 |
89 |
10 × 5 |
250 x 125 |
273.0 |
141.3 |
178 |
|
2 1/2 x 1 1/4 |
65 ×32 |
73.0 |
42.2 |
89 |
10 × 4 |
250 ×100 |
273.0 |
114.3 |
178 |
|
2 1/2 × 1 |
65 ×25 |
73.0 |
33.4 |
89 |
12 × 10 |
300 ×250 |
323.8 |
273.0 |
203 |
|
3 ×2 1/2 |
80 ×65 |
88.9 |
73.0 |
89 |
12 × 8 |
300 ×200 |
323.8 |
219.1 |
203 |
|
3 × 2 |
80 ×50 |
88.9 |
60.3 |
89 |
12 × 6 |
300 ×150 |
323.8 |
168.3 |
203 |
|
3 × 1 1/2 |
80 ×40 |
88.9 |
48.3 |
89 |
12 × 5 |
300 ×125 |
323.8 |
141.3 |
203 |
|
3 × 1 1/4 |
80 ×32 |
88.9 |
42.2 |
89 |
14 × 12 |
350 ×300 |
355.6 |
323.8 |
330 |
|
3 1/2 × 3 |
90 ×80 |
101.6 |
88.9 |
102 |
14 × 10 |
350 ×250 |
355.6 |
273.0 |
330 |
|
3 1/2 x 2 1/2 |
90 ×65 |
101.6 |
73.0 |
102 |
14 × 8 |
350 ×200 |
355.6 |
219.1 |
330 |
|
3 1/2 × 2 |
90 ×50 |
101.6 |
60.3 |
102 |
14 × 6 |
350 ×150 |
355.6 |
168.3 |
330 |
|
3 1/2 × 1 1/2 |
90 ×40 |
101.6 |
48.3 |
102 |
16 × 14 |
400 ×350 |
406.4 |
355.6 |
356 |
|
3 1/2 x 2 1/4 |
90 ×32 |
101.6 |
42.2 |
102 |
16 × 12 |
400 ×300 |
406.4 |
323.8 |
356 |
|
4 × 3 1/2 |
100 ×90 |
114.3 |
101.6 |
102 |
16 × 10 |
400 ×250 |
406.4 |
273.0 |
356 |
|
4 × 3 |
100 ×80 |
114.3 |
88.9 |
102 |
16 × 8 |
400 ×200 |
406.4 |
219.1 |
356 |
|
4 × 2 1/2 |
100 ×65 |
114.3 |
73.0 |
102 |
18 × 16 |
450 ×400 |
457 |
406.4 |
381 |
|
4 × 2 |
100 ×50 |
114.3 |
60.3 |
102 |
18 × 14 |
450 ×350 |
457 |
355.6 |
381 |
|
4 ×1 1/2 |
100 ×40 |
114.3 |
48.3 |
102 |
18 × 12 18 × 10 |
450 ×300 450 ×250 |
457 457 |
323.8 273.0 |
381 381 |
Dimansyon Reyon Long-Redui Koud yo
|
Nominal Tiyo Gwosè (NPS) |
DN |
Dyamèt deyò nan Bevel |
Sant- pou -fen, A |
Nominal Tiyo Gwosè (NPS) |
DN |
Dyamèt deyò nan Bevel |
Sant- pou -fen, A |
||
|
Gwo fen |
Ti fen |
Gwo fen |
Ti fen |
||||||
|
2 × 1 1/2 |
50 × 40 |
60.3 |
48.3 |
76 |
10 × 8 |
250 × 200 |
273.0 |
219.1 |
381 |
|
2 × 1 1/4 |
50 × 32 |
60.3 |
42.2 |
76 |
10 × 6 |
250 × 150 |
273.0 |
168.3 |
381 |
|
2 × 1 |
50 × 25 |
60.3 |
33.4 |
76 |
10 × 5 |
250 × 125 |
273.0 |
141.3 |
381 |
|
2 1/2 × 2 |
65 × 50 |
73.0 |
60.3 |
95 |
12 × 10 |
300 × 250 |
323.8 |
273.0 |
457 |
|
2 1/2 × 1 1/2 |
65 × 40 |
73.0 |
48.3 |
95 |
12 × 8 |
300 × 200 |
323.8 |
219.1 |
457 |
|
2 1/2 × 1 1/4 |
65 × 32 |
73.0 |
42.2 |
95 |
12 × 6 |
300 × 150 |
323.8 |
168.3 |
457 |
|
3 × 2 1/2 |
80 × 65 |
88.9 |
73.0 |
114 |
14 × 12 |
350 × 300 |
355.6 |
323.8 |
533 |
|
3 × 2 |
80 × 50 |
88.9 |
60.3 |
114 |
14 × 10 |
350 × 250 |
355.6 |
273.0 |
533 |
|
3 × 1 1/2 |
80 × 40 |
88.9 |
48.3 |
114 |
14 × 8 |
350 × 200 |
355.6 |
219.1 |
533 |
|
3 1/2 × 3 |
90 × 80 |
101.6 |
88.9 |
133 |
16 × 14 |
400 × 350 |
406.4 |
355.6 |
610 |
|
3 1/2 × 2 1/2 |
90 × 65 |
101.6 |
73.0 |
133 |
16 × 12 |
400 × 300 |
406.4 |
323.8 |
610 |
|
3 1/2 × 2 |
90 × 50 |
101.6 |
60.3 |
133 |
16 × 10 |
400 × 250 |
406.4 |
273.0 |
610 |
|
4 × 3 1/2 |
100 × 90 |
114.3 |
101.6 |
152 |
18 × 16 |
450 × 400 |
457 |
406.4 |
686 |
|
4 × 3 |
100 × 80 |
114.3 |
88.9 |
152 |
18 × 14 |
450 × 350 |
457 |
355.6 |
686 |
|
4 × 2 1/2 |
100 × 65 |
114.3 |
73.0 |
152 |
18 × 12 |
450 × 300 |
457 |
323.8 |
686 |
|
4 × 2 |
100 × 50 |
114.3 |
60.3 |
152 |
18 × 10 |
450 × 250 |
457 |
273.0 |
686 |
|
5 × 4 |
125 × 100 |
141.3 |
114.3 |
190 |
20 × 18 |
500 × 450 |
508 |
457 |
762 |
|
5 × 3 1/2 |
125 × 90 |
141.3 |
101.6 |
190 |
20 × 16 |
500 × 400 |
508 |
406.4 |
762 |
|
5 × 3 |
125 × 80 |
141.3 |
88.9 |
190 |
20 × 14 |
500 × 350 |
508 |
355.6 |
762 |
|
5 × 2 1/2 |
125 × 65 |
141.3 |
73.0 |
190 |
20 × 12 |
500 × 300 |
508 |
323.8 |
762 |
|
6 × 5 |
150 × 125 |
168.3 |
141.3 |
229 |
20 × 10 |
500 × 250 |
610 |
273.0 |
762 |
|
6 × 4 |
150 × 100 |
168.3 |
114.3 |
229 |
24 × 22 |
600 × 550 |
610 |
559 |
914 |
|
6 × 3 1/2 |
150 × 90 |
168.3 |
101.6 |
229 |
24 × 20 |
600 × 500 |
610 |
508 |
914 |
|
6 × 3 |
150 × 80 |
168.3 |
88.9 |
229 |
24 × 18 |
600 × 450 |
610 |
457 |
914 |
|
8 × 6 |
200 × 150 |
219.1 |
168.3 |
305 |
24 × 16 |
600 × 400 |
610 |
406.4 |
914 |
|
8 × 5 |
200 × 125 |
219.1 |
141.3 |
305 |
24 × 14 |
600 × 350 |
610 |
355.6 |
914 |
|
8 × 4 |
200 × 100 |
219.1 |
114.3 |
305 |
24 × 12 |
600 × 300 |
610 |
323.8 |
914 |
Dimansyon nan koud long reyon
|
Gwosè tiyo nominal (NPS) |
DN |
Deyò Dyamèt nan Bevel |
Sant-pou-Fen |
|
|
90 degre Koud, A |
45 degre Koud, B |
|||
|
1/2 |
15 |
21.3 |
38 |
16 |
|
3/4 |
20 |
26.7 |
38 |
19 |
|
1 |
25 |
33.4 |
38 |
22 |
|
1 1/4 |
32 |
42.2 |
48 |
25 |
|
1 1/2 |
40 |
48.3 |
57 |
29 |
|
2 |
50 |
60.3 |
76 |
35 |
|
2 1/2 |
65 |
73.0 |
95 |
44 |
|
3 |
80 |
88.9 |
114 |
51 |
|
3 1/2 |
90 |
101.6 |
133 |
57 |
|
4 |
100 |
114.3 |
152 |
64 |
|
5 |
125 |
141.3 |
190 |
79 |
|
6 |
150 |
168.3 |
229 |
95 |
|
8 |
200 |
219.1 |
305 |
127 |
|
10 |
250 |
273.0 |
381 |
159 |
|
12 |
300 |
323.8 |
457 |
190 |
|
14 |
350 |
355.6 |
533 |
222 |
|
16 |
400 |
406.4 |
610 |
254 |
|
18 |
450 |
457 |
686 |
286 |
|
20 |
500 |
508 |
762 |
318 |
|
22 |
550 |
559 |
838 |
343 |
|
24 |
600 |
610 |
914 |
381 |
|
26 |
650 |
660 |
991 |
405 |
|
28 |
700 |
711 |
1067 |
438 |
|
30 |
750 |
762 |
1143 |
470 |
|
32 |
800 |
813 |
1219 |
502 |
|
34 |
850 |
864 |
1295 |
533 |
|
36 |
900 |
914 |
1372 |
565 |
|
38 |
950 |
965 |
1448 |
600 |
|
40 |
1000 |
1016 |
1524 |
632 |
|
42 |
1050 |
1067 |
1600 |
660 |
|
44 |
1100 |
1118 |
1676 |
695 |
|
46 |
1150 |
1168 |
1753 |
727 |
|
48 |
1200 |
1219 |
1829 |
759 |
Dimansyon Lap Joint Stub Ends
|
Nominal Tiyo Gwosè(NPS) |
DN |
Deyò Dyamèt nan Barik |
Long Modèl Longè, F[Nòt (3), (4)] |
Kout Modèl Longè, F[Nòt (3), (4)] |
Reyon nan Filet, R[Remak (5)] |
Dyamèt nan Wis, G[Remak (6)] |
|
|
Max. |
Min. |
||||||
|
1/2 |
15 |
22.8 |
20.5 |
76 |
51 |
3 |
35 |
|
3/4 |
20 |
28.1 |
25.9 |
76 |
51 |
3 |
43 |
|
1 |
25 |
35.0 |
32.6 |
102 |
51 |
3 |
51 |
|
1 1/4 |
32 |
43.6 |
41.4 |
102 |
51 |
5 |
64 |
|
1 1/2 |
40 |
49.9 |
47.5 |
102 |
51 |
6 |
73 |
|
2 |
50 |
62.4 |
59.5 |
152 |
64 |
8 |
92 |
|
2 1/2 |
65 |
75.3 |
72.2 |
152 |
64 |
8 |
106 |
|
3 |
80 |
91.3 |
88.1 |
152 |
64 |
10 |
127 |
|
3 1/2 |
90 |
104.0 |
100.8 |
152 |
76 |
10 |
140 |
|
4 |
100 |
116.7 |
113.5 |
152 |
76 |
11 |
157 |
|
5 |
125 |
144.3 |
140.5 |
203 |
76 |
11 |
185 |
|
6 |
150 |
171.3 |
167.5 |
203 |
89 |
13 |
218 |
|
8 |
200 |
222.1 |
218.3 |
203 |
102 |
13 |
270 |
|
10 |
250 |
277.2 |
272.3 |
254 |
127 |
13 |
324 |
|
12 |
300 |
328.0 |
323.1 |
254 |
152 |
13 |
381 |
|
14 |
350 |
359.9 |
354.8 |
305 |
152 |
13 |
413 |
|
16 |
400 |
411.0 |
405.6 |
305 |
152 |
13 |
470 |
|
18 |
450 |
462 |
456 |
305 |
152 |
13 |
533 |
|
20 |
500 |
514 |
507 |
305 |
152 |
13 |
584 |
|
22 |
550 |
565 |
558 |
305 |
152 |
13 |
641 |
|
24 |
600 |
616 |
609 |
305 |
152 |
13 |
692 |
Dimansyon nan bouchon
|
Nominal Gwosè tiyo (NPS) |
DN |
Deyò Dyamèt nan Bevel |
Longè, E [Remak (1)] |
Limite miray la Epesè pou Longè, E |
Longè, E [Remak (2)] |
|
1/2 3/4 1 1 1/4 1 1/2 2 2 1/2 3 3 1/2 4 5 6 8 10 12 14 16 18 20 22 24 26 28 30 32 34 36 38 40 42 44 46 48 |
15 20 25 32 40 50 65 80 90 100 125 150 200 250 300 350 400 450 500 550 600 650 700 750 800 850 900 950 1000 1050 1100 1150 1200 |
21.3 26.7 33.4 42.2 48.3 60.3 73.0 88.9 101.6 114.3 141.3 168.3 219.1 273.0 323.8 355.6 406.4 457 508 559 610 660 711 762 813 864 914 965 1016 1067 1118 1168 1219 |
25 25 38 38 38 38 38 51 64 64 76 89 102 127 152 165 178 203 229 254 267 267 267 267 267 267 267 305 305 305 343 343 343 |
4.57 3.81 4.57 4.83 5.08 5.59 7.11 7.62 8.13 8.64 9.65 10.92 12.70 12.70 12.70 12.70 12.70 12.70 12.70 12.70 12.70 . . . . . . . . . . . .
. . . . . . . . . . . . . . .
. . . . . . . . . |
25 25 38 38 38 44 51 64 76 76 89 102 127 152 178 191 203 229 254 254 305 . . . . . . . . . . . .
. . . . . . . . . . . . . . .
. . . . . . . . . |
Konklizyon
Mwen espere gid detaye sa a itil pou bezwen akizisyon ou ak jeni. Pou plis detay spesifikasyon, èske w ta enterese nan yon dekonpozisyon pi detaye nan evalyasyon presyon-tanperati pou diferan orè nan ekipman 254SMO?