316LN (UNS S31653, EN 1.4406 / 1.4429)se yon vèsyon nitwojèn-alye, ba-kabòn nan asye pur austenitic 316L klasik la.

"N" vle di adisyon entansyonèl nan nitwojèn, ki siyifikativman amelyore fòs mekanik pandan y ap konsève ekselan rezistans korozyon ak soudabilite ki fè 316 la.

 

316LN Stainless Steel Properties

 

316LN NerjaveèiKonpozisyon chimiksou

 

Eleman

316LN (1.4406)

316LN (1.4429 pi wo-Mo)

C

Mwens pase oswa egal a 0.030

Mwens pase oswa egal a 0.030

Kr

16.5–18.5

16.5–18.5

Ni

10.0–13.0

11.0–14.0

Mo

2.00–2.50

2.50–3.00

N

0.10–0.16

0.12–0.22

Mn

Mwens pase oswa egal a 2.00

Mwens pase oswa egal a 2.00

Si

Mwens pase oswa egal a 1.00

Mwens pase oswa egal a 0.70

P, S

Trè ba

Trè ba

 

Azòt ki pi wo a ak opsyonèl pi wo Variant molybdène (1.4429) delivre menm pi bon rezistans korozyon pitting ak crevice.

 

316LN NerjaveèiPwopriyete mekanik

 

Pwopriyete

Valè (tipik)

Creole / Nòt

Fòs rupture (Rm)

580-800 MPa

Pi wo pase 316L (Pi wo pase oswa egal a 520 MPa)

Fòs Sede (Rp0.2)

Pi gran pase oswa egal a 260-300 MPa

~ 40-50% pi fò pase 316L

elongasyon (A5)

Pi gran pase oswa egal a 40-45%

Ekselan duktilite

Dite

Mwens pase oswa egal a 215 HB / Mwens pase oswa egal a 95 HRB

 

Severite enpak (Charpy V, 20 degre)

>100 J (souvan > 150 J)

Rete wo menm nan -196 degre

Modil Elastisite

200 GPa (20 degre)

Diminye a ~ 186 GPa nan 200 degre

 

Efè ranfòsman nitwojèn pèmèt 316LN yo dwe itilize nan pi wo -aplikasyon estrès oswa pèmèt rediksyon pwa nan mi mens pandan y ap kenbe ekivalan chaj-kapasite pote konpare ak 316L.

 

316LN NerjaveèiPwopriyete Fizik

 

Pwopriyete

Valè

Dansite

8.00 g/cm³

Kondiktivite tèmik

15 W/m·K

Kapasite Chalè Espesifik

500 J/kg·K

Koefisyan ekspansyon tèmik

16.0 × 10⁻⁶/K (20-100 degre)

Rezistivite elektrik

0.75 Ω·mm²/m

Ranje k ap fonn

1375-1400 degre

Pèmeyabilite mayetik

Mwens pase oswa egal a 1.005 (esansyèlman ki pa-mayetik nan eta rkwit)

 

316LN Nerjaveèi asye korozyon rezistans

 

316LN Stainless Steel Corrosion Resistance

 

General & Pitting/Crevice Corrosion: The combination of molybdenum and nitrogen provides outstanding resistance to a wide range of chemical corrodents, including chlorides found in marine and chemical processing environments. Its PREN (Cr% + 3.3Mo% + 16N%) is typically >28.

 

Intergranular Kowozyon: "LN" konbinezon an patikilyèman efikas. Ultra-kabòn ki ba minimize fòmasyon carbure, pandan y ap nitwojèn amelyore estabilite mikwostrikti a nan zòn chalè-afèkte soude yo, sa ki fè li yon chwa ekselan pou ekipman fabrike ki pa ka rkwit apre-soude.

 

316LN NerjaveèiKarakteristik fabrikasyon ak soude

 

316LN se jeneralman soude pa tout metòd fizyon estanda. Sepandan, pi gwo fòs li yo ak to redi travay mande pou konsiderasyon:

 

Soude:Ekselan soudabilite. Pwosesis komen yo enkli TIG, MIG, ak SAW. Pa gen tretman chalè post-soude nòmalman obligatwa. Yo rekòmande pou sèvi ak metal ranpli matche oswa plis -alliye.

 

Machining:Pi gwo fòs li yo ak tandans travay -redi nan rezilta nan yon evalyasyon machinabilite pi ba konpare ak 304 oswa 316L. Sèvi ak konfigirasyon rijid, zouti rato pozitif, ak likid refwadisman apwopriye.

 

Travay frèt:Duktilite ekselan pèmèt pou gwo operasyon frèt fòme. Sepandan, pi wo fòs yo mande yo, ak to a ogmante travay di ka nesesite etap rkwir entèmedyè pou deformation grav.

 

Konklizyon

 

316LN konbine rezistans korozyon pwouve nan fanmi 316 la ak fòs mekanik siyifikativman pi wo ak rezistans amelyore nan twou ak krak korozyon estrès, tout pandan y ap kenbe soudabilite eksepsyonèl ak ba -tanperati severite.

 

Kòm yon manifakti pwofesyonèl tiyo asye pur ak anpil eksperyans nan 316LN fòje bride, ekipman soude bou, ak sistèm tiyo san pwoblèm / soude, nou kenbe stock pare epi ofri sètifika tès materyèl an akò strik ak EN 10204.

 

Kontakte ekip teknik lavant nou anpou sitasyon pi ba sou ekipman 316LN ak bride.

 

Voye rechèch
Vin jwenn nou
Epi kòmanse RFQs ou kounye a.
Kontakte nou